It should be remembered that accelerators containing chlorine do not admit of a great change of color of coating on the plate. Iodide of Starch. This mixture can be employed for coating over in warm weather, and prevent the flashing resulting at high temperatures. It may be used the same as the iodide alone. To six ounces of finely pulverized starch, add one fourth ounce of dry iodine. Use.
Practise has proved that but a slight variation in the chemical coating, of the Daguerreotype plate will very materially affect the final result. The operator will proportion the coating of iodine and bromine or accelerators according to the strength and composition of the latter.